Effect of different high‐palladium metal‐ceramic alloys on the color of opaque porcelain
Authors:
- Minos M. StavridakisMSMinos M. Stavridakis
- Efstratios PapazoglouEPEfstratios Papazoglou
- Robert R. SeghiRSRobert R. Seghi
- William M. JohnstonWJWilliam M. Johnston
- 1 June 2000
- journal article
- Published by Wiley in Journal of Prosthodontics
- Vol. 9 (2) , 71-76
Abstract
Purpose The purpose of this study was to assess the effect of different high‐palladium alloys on the resulting color of opaque porcelain. Three Pd‐Cu‐Ga alloys, Spartan Plus (S; Williams Dental Co/Division of Ivoclar North America, Amhest, NY), Liberty (B; J.F. Jelenko & Co, Armonk, NY), and Freedom Plus (F; J.F. Jelenko & Co); 4 Pd‐Ga alloys, Legacy (L; J.F. Jelenko & Co), IS 85 (I; Williams Dental Co), Protocol (P; Williams Dental Co), and Legacy XT (X; J.F. Jelenko & Co); and a Pd‐Ag alloy, Super Star (T; J.F. Jelenko & Co), were examined. The Au‐Pd alloy Olympia (O; J.F. Jelenko & Co) served as the control.Materials and Methods Three cast 16‐mm discs, 1‐mm thick, were prepared from each of the alloys. After metallurgically polishing and air‐abrading, the specimens were oxidized following the manufacturer's recommendations. Shade B1 opaque porcelain (Vita‐Omega; Vident, Baldwin Park, CA) was applied at a final thickness of 0.1 mm using a mold. After 2 opaque porcelain firing cycles, the surfaces were air‐abraded. The colors of the specimens were measured using a colorimeter and expressed in Commission International de l'Eclairage (CIE) L*a*b* coordinates. Color differences (ΔE) were determined between the control and each experimental group. Analysis of Variance and Tukey‐Kramer tests were performed on the ΔE data.Results The 3 Pd‐Cu‐Ga alloys showed significantly greater (p < .01) ΔE values (S = 2.8 ± 1.1, B = 3.0 ± 0.6, and F = 2.1 ± 0.2) than the remaining 5 experimental groups (L = 0.7 ± 0.5, I = 0.7 ± 0.4, P = 0.7 ± 0.2, X = 0.7 ± 0.4, and T = 0.7 ± 0.5). The directions of the significant color changes were relatively equally distributed along the L*, a*, and b* axes, and all ΔL*, Δa*, and Δb* values were negative (lower value, more green and blue relative to control O).Conclusions This work suggests that a 0.1‐mm‐thick layer of opaque porcelain in the Pd‐Cu‐Ga alloys studied, did not reliably reproduce the color of porcelain.Keywords
This publication has 8 references indexed in Scilit:
- Spectrophotometric analysis of a nongreening, metal-fusing porcelainThe Journal of Prosthetic Dentistry, 1991
- Effect of different metal ceramic alloys on the color of opaque and dentin porcelainThe Journal of Prosthetic Dentistry, 1991
- Visual and Instrumental Colorimetric Assessments of Small Color Differences on Translucent Dental PorcelainJournal of Dental Research, 1989
- Performance Assessment of Colorimetric Devices on Dental PorcelainsJournal of Dental Research, 1989
- The effects of manipulative variables on the color of ceramic metal restorationsThe Journal of Prosthetic Dentistry, 1988
- Effect of porcelain thickness and type of metal-ceramic alloy on colorThe Journal of Prosthetic Dentistry, 1987
- Spectrophotometric analysis of color differences between porcelain systemsThe Journal of Prosthetic Dentistry, 1986
- Spectrophotometric study of five porcelain shades relative to the dimensions of color, porcelain thickness, and repeated firingsThe Journal of Prosthetic Dentistry, 1979