Effect of Chemical Composition on the Sinterability of Ultrafine Sic Powders

Authors:

Abstract
Ultrafine β‐SiC powders with an average particle size of 0.01 to 0.06 μm were produced by CVD methods. When these powders contained enough carbon to remove impurity oxygen, sintered bodies with a relative density >95% were uchieved at 2050°C in the presence of 1 wt% boron. The Vickers microhardness reached 21 to 25 GPa at a density of ∼95% .