Abstract
The aging behavior of 3 mol% Nb2O5Pb(Zr0.52Ti0.48)O3with addition of 0.1–3 mol% Cr2O3prepared via the solid-state reaction technique have been investigated. The aging rate increased with increasing Cr concentration from 0.1 to 0.6 mol%. Further increase in Cr concentration, the aging rate decreased dramatically. From ferroelectric hysteresis loops measurements, the decrease of polarization existed in all of concentrations.