Abstract
Heat-treatable AA6061-T6 weldability leads to a decline in the physio-mechanical and tribological properties due to strengthening precipitates dissolution in the nugget zone of FS-welded joints. Improvement in these properties is governed by reinforcement particles addition in the weld joint line for non-heat treatable Al-alloys. Although, its application to AA6061-T6 is scant. In the present work, FS-welded joints were produced by reinforcing Al 2 O 3 nanoparticles into the faying surface of the base matrix. The purpose of Al 2 O 3 nanoparticles addition is to refine the microstructure of the nugget zone and to obstruct the granular growing in the heat-affected zone. FSW was conducted at constant rotating 2000 rpm, transverse 70 mm min −1 speed to illustrate the influence of Al 2 O 3 addition on mechanical, microstructure, micro-hardness, and wear properties of welds compared to parent alloy and unreinforced joints. Findings revealed that Al 2 O 3 nanoparticles addition along the joint line leads to noteworthy grains refinement structure of weld zone (6 μ m) compared with the base material (38 μ m) and unreinforced nugget (18 μ m) joints. In addition, reinforced FS-W nugget zone have banded structure of alternate regions namely, nanoparticles-rich and free those have a difference in grain size, such that, the nanoparticle-rich region has fine grain size (6 μ m) than nano particle-free (14 μ m) region. Due to Zener-influence occurred via Al 2 O 3 nanoparticles helps to avoid the grain growth accompanied by dynamic recrystallization throughout FSW process which results in granular size reduction. Tensile strength (246 MPa/73%), microhardness (88HV/52%), and wear properties was notably increased for reinforced FSW joint compared to unreinforced joint (tensile strength (180MPa), micro-hardness (46 HV), and lower wear resistance, under similar parameters which attribute to nanoparticles presence in processed area. Moreover, single FSW pass leads to non-uniform distribution of Al 2 O 3 nanoparticles and nucleation of voids at Al/Al 2 O 3 boundary in the heat-affected zone which leads to early fracture of welded joint during tensile loading.

This publication has 37 references indexed in Scilit: