Visualizing the Carbon Binder Phase of Battery Electrodes in Three Dimensions
Open Access
- 20 July 2018
- journal article
- research article
- Published by American Chemical Society (ACS) in ACS Applied Energy Materials
- Vol. 1 (8) , 3702-3710
Abstract
This study presents a technique to directly characterize the carbon and binder domain (CBD) in lithium-ion (Li-ion) battery electrodes in three dimensions and use it to determine the effective transport properties of a LiNi0.33Mn0.33Co0.33O2 (NMC) electrode. X-ray nanocomputed tomography (nano-CT) is used to image an electrode composed solely of carbon and binder, whereas focused ion beam–scanning electron microscopy is used to analyze cross-sections of a NMC electrode to gain morphological information regarding the electrode and CBD porosity. Combining the information gathered from these techniques reduces the uncertainty inherent in segmenting the nano-CT CBD data set and enables effective diffusivity of its porous network to be determined. X-ray microcomputed tomography (micro-CT) is then used to collect a NMC data set that is subsequently segmented into three phases, comprised of active material, pore, and CBD. The effective diffusivity calculated for the nano-CT data set is incorporated for the CBD present in the micro-CT data set to estimate the ensemble tortuosity factor for the NMC electrode. The tortuosity factor greatly increases when compared to the same data set segmented without considering the CBD. The porous network of the NMC electrode is studied with a continuous pore size distribution approach that highlights median radii of 180 nm and 1 μm for the CBD and NMC pores, respectively, and with a pore throat size distribution calculation that highlights median equivalent radii of 350 and 700 nm.Keywords
Funding Information
- Engineering and Physical Sciences Research Council (EP/M009394/1, EP/K005030/1, EP/N032888/1)
- Royal Academy of Engineering
This publication has 43 references indexed in Scilit:
- Three Dimensional Simulation of Galvanostatic Discharge of LiCoO2Cathode Based on X-ray Nano-CT ImagesJournal of the Electrochemical Society, 2012
- In situ scanning electron microscopy on lithium-ion battery electrodes using an ionic liquidJournal of Power Sources, 2011
- Local Tortuosity Inhomogeneities in a Lithium Battery Composite ElectrodeJournal of the Electrochemical Society, 2011
- X-ray microtomographyMaterials Characterization, 2010
- Characterization of the 3-dimensional microstructure of a graphite negative electrode from a Li-ion batteryElectrochemistry Communications, 2010
- Quantifying tortuosity in porous Li-ion battery materialsJournal of Power Sources, 2009
- Contradicting Geometrical Concepts in Pore Size Analysis Attained with Electron Microscopy and Mercury IntrusionJournal of the American Ceramic Society, 2008
- X-ray nanotomographyMaterials Today, 2007
- Modeling of Galvanostatic Charge and Discharge of the Lithium/Polymer/Insertion CellJournal of the Electrochemical Society, 1993
- Practical cone-beam algorithmJournal of the Optical Society of America A, 1984