A coating of barium hexaaluminate (Ba 0.75 Al 11.0 O 17.25 ) on an α‐SiC substrate and the thermal stability of the formed film were investigated for a high‐temperature catalytic application. The film prepared by sol coating consisted of BaAl 2 Si 2 O 8 and α‐Al 2 O 3 phases and always contained many cracks or exfoliations after heating at 1200C. A hexaaluminate porous film was successfully formed by slurry coating without void formation at the interface between the film and the substrate and exfoliation due to the formation of the intermediate layer after heating at 1200°C. The microstructure of the film remained unchanged, even after heating at 1300°C.