Comparative study of ceramic-to-metal bonding
Open Access
- 1 January 2007
- journal article
- research article
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 18 (3) , 240-243
Abstract
Dentists and technicians have used dental ceramics associated with different types of alloys without taking into account the characteristics of compatibility of these materials. Knowing the properties of the alloy and ceramic used in metal/ceramic restorations is a key factor for treatment success. The purpose of this study was to evaluate the bond strength of a palladium-silver alloy (Pors-on 4) to 3 ceramics (Ceramco, Noritake and Vita VMK-68) using shear forces at the metal-ceramic interface. A stainless steel cylindrical matrix was used for preparation of the metal dies, application of ceramic and shear strength testing. Thirty palladium-silver alloy cylinders received two layers of opaque and two layers of body porcelain, and shear tests were performed in a universal testing machine at a cross-head speed of 0.5 mm/min. Shear bond strength means (in MPa) were: 28.21(Ceramco), 28.96 (Noritake) and 24.11 (Vita VMK-68). One-way ANOVA did not show statistically significant differences (p>0.05) among the materials. The results of this study indicate that the three evaluated ceramic systems are suitable to be used in combination with the tested palladium-silver alloy.Keywords
This publication has 16 references indexed in Scilit:
- Influence of casting procedures on the corrosion resistance of clinical dental alloys containing palladium☆Acta Biomaterialia, 2006
- Spectrophotometric evaluation of the optical influence of different metal alloys and porcelains in the metal-ceramic complexThe Journal of Prosthetic Dentistry, 2004
- Designs of bond strength tests for metal-ceramic complexes: Review of the literatureThe Journal of Prosthetic Dentistry, 1996
- The effect of oxidation heat treatment on porcelain bond strength in selected base metal alloysThe Journal of Prosthetic Dentistry, 1991
- Oxidation of four palladium-rich ceramic fusing alloysBiomaterials, 1990
- Carbon impurities and properties of some palladium alloys for ceramic veneeringDental Materials, 1985
- High-temperature Behavior of a Pd-Ag Alloy for PorcelainJournal of Dental Research, 1983
- A simple shear test to evaluate the bond strength of ceramic fused to metalAustralian Dental Journal, 1980
- The strength of metal-ceramic bonds with base metals containing chromium. A preliminary reportBritish Dental Journal, 1972
- Porcelain baked to gold—A new medium in prosthodonticsThe Journal of Prosthetic Dentistry, 1956