Effect of boric anhydride on viscosity of slags used in electric melting of metallized siderite concentrate
Open Access
- 11 November 2023
- journal article
- research article
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (5) , 597-603
Abstract
The Bakal deposit located in the Southern Urals near the city of Bakal, Chelyabinsk region, is one of the largest deposits of carbonate iron ores (siderites). The total deposit of siderites is about 1 billion tons. They are not in demand among metallurgists because of their low iron content and high magnesium content. At the same time, the Urals metallurgical enterprises are suffering from shortage of iron ore raw materials including steelmaking ore raw materials. The high purity of siderites in terms of phosphorus and non-ferrous metals makes it possible to use methods of coke-free metallurgy for their processing. Pyrometallurgical processing of siderites including their reduction roasting in a rotary furnace followed by grinding and magnetic separation allows obtaining a concentrate to be used as a steelmaking raw material having metallization degree above 90 % and a waste rock content under 3 – 7 %. Calculations showed that the costs of electricity used for melting scrap metal and metallized siderite concentrate containing 30 % of waste rock and loaded into the furnace at temperatures above 1000 °C are close. We propose a siderite processing method including reduction of the initial ore in a rotary furnace, and melting of resulting metallized concentrate hot loaded (at temperatures above 1000 °C) into a furnace. The empty rock of metallized siderite concentrate contains a large percentage of magnesium oxide that makes it refractory. To obtain liquid slag, it is proposed to add boric anhydride in the form of colemanite. To assess the B2O3 effect on melting of the metallized siderite oxide phase in the process of electric melting, studies on the viscosity correlation of the magnesian steelmaking slag containing B2O3 with temperature and its composition were carried out. It was found that at the discharge temperature (1600 °C) the resulting magnesia slag with the ratio of MgO/SiO2 in the initial siderite equaling to 0.75 – 1.25 has a low viscosity (less than 3.65 P).Keywords
This publication has 9 references indexed in Scilit:
- Structure Sensitive Properties of System B2O3- CaO MeltsDefect and Diffusion Forum, 2020
- Elaboration of an environmentally appropriate technology of siderite ores concentrationFerrous Metallurgy. Bulletin of Scientific , Technical and Economic Information, 2019
- Aragonite–calcite veins of the ‘Erzberg’ iron ore deposit (Austria): Environmental implications from young fracturesSedimentology, 2018
- Influence of B2O3 on Viscosity of High Ti-bearing Blast Furnace SlagISIJ International, 2012
- Catalyzing Carbothermic Reduction of Siderite Ore with High Content of Phosphorus by Adding Sodium CarbonateISIJ International, 2011
- Organic and inorganic geochemistry of Ljubija siderite deposits, NW Bosnia and HerzegovinaMineralium Deposita, 2009
- The role of organic matter in the formation of siderite from Xuanlong area, Hebei ProvinceChinese Journal of Geochemistry, 1997
- Strontium isotopic evidence for the origin of siderite, ankerite and magnesite mineralizations in the Eastern AlpsMineralium Deposita, 1988
- Composition of siderite and the environments of formation of vein-type deposits in JapanEconomic Geology, 1977