Thermoelectric Properties of Bi2Te3/Sb2Te3 Thin Films
- 15 May 2006
- journal article
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 514-516, 156-160
Abstract
The deposition and characterization of n-type Bi2Te3 and p-type Sb2Te3 semiconductor films are reported. The films were deposited by thermal co-evaporation on a 25 µm thick polyimide (kapton) substrate. The co-evaporation method is inexpensive, simple, and reliable, when compared to other techniques that need longer time periods to prepare the starting material or require more complicated and expensive deposition equipment. Seebeck coefficients of -189 µVK-1 and +140 µVK-1 and electrical resistivities of 7.7 µ0m and 15.1 µ0m were measured at room temperature on n-type and p-type films, respectively. These values are better than those reported for films deposited by co-sputtering or electrochemical deposition, and are close to those reported for films deposited by metal-organic chemical vapour deposition or flash evaporation. Because of their high figures of merit, these films will be used for the fabrication of a micro-Peltier element, useful in temperature control and laser-cooling for telecommunications.Keywords
This publication has 8 references indexed in Scilit:
- New thermoelectric components using microsystem technologiesJournal of Microelectromechanical Systems, 2004
- Thermoelectric microdevice fabrication process and evaluation at the Jet Propulsion Laboratory (JPL)2003
- Peltier effect in a co-evaporated Sb2Te3(P)-Bi2Te3(N) thin film thermocoupleThin Solid Films, 2002
- Miniaturized Thermoelectric Cooler2002
- Thin-film thermoelectric devices with high room-temperature figures of meritNature, 2001
- Growth of Bi2Te3 and Sb2Te3 thin films by MOCVDMaterials Science and Engineering: B, 1999
- Cooling performance of integrated thermoelectric microcoolerSolid-State Electronics, 1999
- Flash evaporated layers of (Bi2Te3–Bi2Se3)(N) and (Bi2Te3–Sb2Te3)(P)Materials Science and Engineering: B, 1998