We show that with increasing magnitude of current (I), insulator-metal (I-M) transition in Sm0.6Sr0.4MnO3 becomes discontinuous and shifts down in temperature, which is accompanied by an abrupt decrease in temperature of the sample while cooling. The I-M transition exhibits a hysteresis while warming. A magnetic field of μ0H=0.5 T results in −99% magnetoresistance for I=11 mA compared to −32% for I=1 mA. Our results underscore the importance of inhomogeneous Joule heating that leads to coexistence of the high temperature paramagnetic phase with the low temperature ferromagnetic phase over a wide temperature range.