Abstract
TiO2 thin films on silicon wafers have been prepared from the reaction of Ti(NMe2)4 with O2 at 250–300 °C by CVD processes. These films, which are carbon free and contain no TiN or TiOxNy species, are amorphous before annealing but crystalline anatase after annealing at 600 °C in air. The average dielectric constant (κ) of the annealed films is 50(5), with an average leakage current of 5(3)×10–5 A cm–2, and breakdown strength of 1.8(0.3) MV cm–1.