WC–CrC–Ni cermet coatings that are sprayed with a high velocity oxygen fuel are widely used on parts requiring abrasive sliding wear resistance such as hydraulic pistons, shafts, and bearings, nevertheless, their characteristics can be modified during exposure to heat. This study applies to an HVOF-deposited WC-CrC-Ni coating which underwent isothermal post-heat treatment and correlates the phase development, hardness, tribology, and corrosion. Scanning electron microscopy was used to investigate the microstructural features, whereas the phase composition and carbide stability was assessed by X-ray diffraction and carbide-retention index. The functional performance was analyzed using Vickers microhardness testing, dry sliding wear in an alumina counterbody, and potentiodynamic polarization in a 0.1N HCl aerated solution. The condition producing the maximum hardness reached 1269 ± 20 HV0.3 and was associated with thermally induced densification of splat boundaries, although phase transformations within the carbide system were also detected. In general, the results provide a basis on how to optimize heat-treatment times to make WC–CrC-Ni coating to have a long service life in thermal fluctuating wear conditions.