Corrosion of High-Temperature Alloys in Chloride-Containing Supercritical Water Oxidation Systems
Authors:
- J. KonysJKJ. Konys
- S. FodiSFS. Fodi
- H. SchmidtHSH. Schmidt
- 1 January 1999
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 55 (1) , 45-51
Abstract
Supercritical water oxidation (SCWO) is a promising and effective method for the oxidation of organic wastes. Its high solubility for organic compounds and its special physical properties (i.e., density and viscosity) result in a key advantage over standard processes such as incineration. During oxidation of chlorine organics, severe corrosion attack of most of the materials has been observed as a result of the formation of hydrochloric acid (HCl). An investigation was conducted of corrosion of high-temperature alloys such as alloy 214 (UNS N07214), alloy 602CA (UNS N06602), alloy G-30 (UNS N06030), alloy 625 (UNS N06625), and alloy 686 (UNS N06686), exposed at 400 bar (40 MPa) and 420°C for 24 h in a dichloromethane (CH2Cl2)/hydrogen peroxide (H2O2) mixture with ~ 2,000 wppm chloride (Cl2). Weight losses of all the samples varied between 1.3 mm/y for alloy G-30 and ~ 31.6 mm/y for alloy 686. Alloy 214 showed increased corrosion for the preoxidized material, whereas the corrosion rate of alloy 602CA was reduced by a factor of three as a result of preoxidation at 900°C prior to SCWO exposure. Analysis revealed that alloy 686 lost most of its nickel down to a depth of ~ 150 μm. Alloy G-30 showed good corrosion behavior as a result of formation of a protective oxide layer during the exposure. The layer was homogeneous, with a thickness of ~ 12 μm, but slight nickel leaching was observed.Keywords
This publication has 7 references indexed in Scilit:
- Corrosion Screening Tests With Ni-Base Alloys in Supercritical Water Containing Hydrochloric Acid and Oxygen1996
- Corrosion Studies in Supercritical Water Oxidation Systems1995
- Corrosion Science, Corrosion Engineering, and Advanced TechnologiesCorrosion, 1995
- Corrosion investigation of multilayered ceramics and experimental nickel alloys in SCWO process environments1995
- Supercritical water oxidation: An emerging technologyJournal of Hazardous Materials, 1992
- Thermodynamic Analysis of Corrosion of Iron Alloys in Supercritical Water1989
- Supercritical Water Destruction of Aqueous WastesHazardous Waste, 1984