Photocatalysts that also adsorb are usually ranked by how much pollutant disappears at the end of a run, a number that says nothing about which of the two processes did the work. We separate the two on a single material family by running a dark stage and an illuminated stage in sequence and following the solution in-line. Niobium oxide with nominal Ce loadings of 1 %–5 % was prepared in one hydrothermal step from ammonium niobate oxalate and cerium nitrate, and tested against 20 mg L−1 tetracycline under 254 nm irradiation. Total removal after 180 min did not differ significantly across the three compositions, at 53.5 ± 0.7 %, 57.1 ± 1.9 % and 54.2 ± 3.2 % for Ce1%–Nb2O5, Ce3%–Nb2O5 and Ce5%–Nb2O5 respectively (Welch p≥0.19). The dark stage did separate them: uptake before illumination was 24.4 ± 0.7 mg g−1, 36.6 ± 0.8 mg g−1 and 27.5 ± 0.4 mg g−1 (p≤0.047 for every pair, n=2), and the apparent first-order constant of the UV stage fell as dark uptake rose (r=−0.90, p=0.014, n=6). Direct photolysis cannot produce that spread, because it would be fastest where the solution is most dilute, and dark uptake was close to its plateau by lamp-on, so the spread is attributable to the solids. Ce loading therefore redistributes removal between dark uptake and the UV stage rather than changing the total, so a fixed-time removal percentage cannot rank these materials, whereas dark-stage uptake separates them.

This publication has 46 references indexed in Scilit: