Abstract
The novel low temperature plasma alloying technique that simultaneously introduces both nitrogen and carbon into the surface of austenitic stainless steel has been used in the past to create a hybrid N-C S-Phase. This S-Phase layer boasts of high hardness and wear resistance without any detriment to corrosion resistance. In this study, the afore mentioned hybrid N-C S-Phase was successfully implemented in the surface of two medical grade austenitic stainless steels: ASTM F138 and F1586. At an optimum process temperature of 430°C a very hard, 20μm precipitate-free S-Phase layer was created. Anodic Polarization tests in Ringer’s solution showed that the corrosion resistance of this layer was similar to that of the untreated alloys. Both dry-wear and corrosion-wear (Ringer’s) behaviour of the surface treated alloys showed an improvement of more than 350% and 40% respectively when compared to the untreated material.

This publication has 7 references indexed in Scilit: