Abstract
To ensure the highest safety standards in modern automobiles, the industry is constantly adopting zero-defect frameworks, such as AEC-Q100, which aims for defective-parts-per-billion (DPPB) or grade-0 level reliability standards in automotive integrated-circuit (IC) packages. Most contemporary wire-bonded packages use either pure copper (Cu) or palladium (Pd)-coated copper (PCC) wires bonded to aluminum (Al) bond pads as interconnections. This choice is made due to their lower cost and superior electrical and mechanical performance, compared to traditional gold wire-based devices. However, these Cu–Al wire-bonded interconnections are prone to ion-induced lift-off/open-circuit corrosion failures when exposed to even trace amounts (− and Br−) contaminants, decreasing device longevity. This study investigates corrosion failure mechanisms in Cu and PCC wire-based devices by subjecting non-encapsulated devices to a highly accelerated aqueous-immersion screening test containing 100 ppm chloride (Cl−), 100 ppm bromide (Br−), and a mixed-ion solution (MX: Cl− + Br−). The screening results indicate that even control PCC-Al devices with a Pd overlayer can be susceptible to Cl− and Br− induced corrosion, with 21 ± 1.6% lift-off failures in MX-solution. In contrast, applying a novel Cu-selective passivation reduced lift-off to 3.3 ± 0.6% and introducing phosphonic-acid-based inhibitor into the MX solution eliminated lift-off failures, demonstrating markedly improved reliability.Keywords
Funding Information
- University of North Texas
This publication has 41 references indexed in Scilit:
- Aqueous phosphonic acid treatments of aluminium: Effect of oxide dissolution and re-oxidation on adsorbate formationApplied Surface Science, 2024
- Corrosion inhibition of copper and aluminium by 2-mercaptobenzimidazole and octylphosphonic acid—Surface pre-treatment and method of film preparationElectrochimica Acta, 2022
- Systematic and collaborative approach to problem solving using X-ray photoelectron spectroscopyApplied Surface Science Advances, 2021
- Corrosion-induced degradation and its mechanism study of Cu–Al interface for Cu-wire bonding under HAST conditionsJournal of Alloys and Compounds, 2020
- Cu-Al interfacial formation and kinetic growth behavior during HTS reliability testJournal of Materials Processing Technology, 2019
- Copper wire interconnect reliability evaluation using in-situ High Temperature Storage Life (HTSL) testsMicroelectronics Reliability, 2014
- Bond reliability under humid environment for coated copper wire and bare copper wireMicroelectronics Reliability, 2011
- Overview of wire bonding using copper wire or insulated wireMicroelectronics Reliability, 2011
- Passivation of aluminum with alkyl phosphonic acids for biochip applicationsApplied Surface Science, 2010
- Adsorption of sodium dodecyl sulfate and sodium dodecyl phosphate at the surface of aluminium oxide studied with AFMCorrosion Science, 2010