Subsecond relaxation of internal field after polarization reversal in congruent LiNbO3 and LiTaO3 crystals
Authors:
- 9 October 2000
- journal article
- Published by AIP Publishing in Applied Physics Letters
- Vol. 77 (15) , 2391-2393
Abstract
We developed an experimental method for measuring subsecond temporal evolution of the internal field after polarization reversal in ferroelectric crystals, congruent and crystals. In each crystal the internal field exhibited two distinct relaxations, suggesting that they originate from two different types of defects. The fast one decays in subsecond range while the slow one lasts over days at room temperature. The subsecond relaxation could be fit to a stretched exponential. This method can be applied to other ferroelectric crystals to investigate the properties of defects.
Keywords
This publication has 13 references indexed in Scilit:
- Nanoscale backswitched domain patterning in lithium niobateApplied Physics Letters, 2000
- Backswitch poling in lithium niobate for high-fidelity domain patterning and efficient blue light generationApplied Physics Letters, 1999
- Switching kinetics of 180° domains in congruent LiNbO3 and LiTaO3 crystalsSolid State Communications, 1998
- Wall velocities, switching times, and the stabilization mechanism of 180° domains in congruent LiTaO3 crystalsJournal of Applied Physics, 1998
- Investigation of ferroelectric coercive field in LiNbO 3Applied Physics A, 1997
- Origin of internal field and visualization of 180° domains in congruent LiTaO3 crystalsJournal of Applied Physics, 1996
- Time dependence of ferroelectric coercive field after domain inversion for lithium-tantalate crystalApplied Physics Letters, 1995
- Defect Structure Model of MgO-Doped LiNbO3Journal of Solid State Chemistry, 1995
- Computer-simulation studies of extrinsic defects incrystalsPhysical Review B, 1991
- Internal bias in ferroelectric ceramics: Origin and time dependenceFerroelectrics, 1988