Formation, Characterization, and Hot Isostatic Pressing of Cr 2 O 3 ‐Doped ZrO 2 (0,3 mol% Y 2 O 3 ) Prepared by Hydrazine Method

Authors:

Abstract
In the ZrO 2 ‐Cr 2 O 3 system, metastable t ‐ZrO 2 solid solutions containing up to 11 mol% Cr 2 O 3 crystallize at low temperatures from amorphous materials prepared by the hydrazine method. The lattice parameter c decreases linearly from 0.5149 to 0.5077 nm with increased Cr 2 O 3 content, whereas the lattice parameter a is a constant value ( a = 0.5077 nm) regardless of the starting composition. At higher temperatures, transformation (decomposition) of the solid solutions proceeds in the following way: t (ss)→ t (ss) + m + Cr 2 O 3 → m + Cr 2 O 3 . Above 11 mol% Cr 2 O 3 addition, c‐ZrO 2 phases are formed in the presence of Cr 2 O 3 . The t ‐ZrO 2 solid solution powders have been characterized for particle size, shape, and surface area. They consist of very fine particles (15–30 nm) showing thin platelike morphology. Dense ZrO 2 (3Y)‐Cr 2 O 3 composite ceramics (∼99.7% of theoretical) with an average grain size of 0.3 μm have been fabricated by hot isostatic pressing for 2 h at 1400°C and 196 MPa. Their fracture toughness increases with increased Cr 2 O 3 content. The highest K Ic value of 9.5 MPa·;m 1/2 is achieved in the composite ceramics containing 10 mol% Cr 2 O 3 .

This publication has 15 references indexed in Scilit: