Abstract
The thermal degradation Processes which occur in poly(phenylenesulfide) (PPS) have been studied by direct pyrolysis‐mass spectrometry (DPMS). The structure of the compounds evolved in the overall temperature range of PPS decomposition (400–700°C) suggests the occurrence of several thermal decomposition steps. At the onset of the thermal degradation (430–450°C) this polymer decomposes with the formation of cyclic oligomers, generated by a simple cylization mechanism either initiated at the—SH end groups or by the exchange between the inner sulfur atoms along the polymer chain. At higher temperature (> 500°C) another decomposition reaction takes over with the formation of aromatic linear thiols. The formation of thiodibenzofuran units by a subsequent dehydrogenation reaction occurs in the temperature range of 550–650°C; in fact, pyrolysis products with a quasi‐ladder structure have also been detected. Ultimately, above 600°C, extrusion of sulfur from the pyrolysis residue occurs with the maximum evolution at the end of decomposition (about 700°C). It appears, therefore, that the residue obtained at high temperature tends to have a crosslinked graphite‐like structure from which the bonded sulfur is extruded. © 1994 John Wiley & Sons, Inc.

This publication has 13 references indexed in Scilit: