Properties of Thin Epitaxial Aerosol MOCVD CeO2 Films Grown on (1102) Sapphire

Authors:

Abstract
We have examined the properties of thin epitaxial CeO2 films prepared by aerosol MOCVD. The films were deposited on (1-102) sapphire at deposition temperatures between 500 °C and 900 °C. The best properties were observed for the film grown at high deposition temperatures. The films have thickness ≈ 0.2 µm and the full width at half maximum of the rocking curve 0.3 ° - 0.4 °. The minimal yield measured by backscattering spectrometry in the channeling mode was 5.5 %, confirming high preferred orientation of the deposited films. The epitaxial character of the CeO2 films was revealed by the measurement of the φ-scan. The aerosol MOCVD CeO2 films were found to be suitable as a buffer layer for a preparation of superconducting high-Tc films. YBa2Cu3O7 superconducting films deposited on the CeO2 / (1-102) sapphire exhibit superconducting transition temperature Tc(R=0) = 86 K