Effect of Pr on properties and Sn whisker growth of Sn‐9Zn‐xPr solder
Authors:
- Songbai XueSXSongbai Xue
- Yifu ShenYSYifu Shen
- Zhengxiang XiaoZXZhengxiang Xiao
- Hong ZhuHZHong Zhu
- Weimin LongWLWeimin Long
- Xinquan YuXYXinquan Yu
- 14 September 2012
- journal article
- research article
- Published by Emerald Publishing in Soldering & Surface Mount Technology
- Vol. 24 (4) , 280-286
Abstract
Purpose: The purpose of this paper is to improve the properties of Sn−9Zn solder, so as to meet the requirements of industrial applications.Design/methodology/approach: The effects of Praseodymium on property and Sn whisker growth under aging treatment in Sn−9Zn lead‐free solder were investigated.Findings: The results indicate that with the addition of rare earth Pr, the wettability and mechanical properties of Sn−9Zn solder were improved. The best wettability and comprehensive property of soldered joint is obtained when the content of Pr is 0.08 wt.%. After aging treatment at 150°C for 360 h, the mechanical properties of Sn−9Zn−0.08Pr decreased but are still obviously higher than that of Sn−9Zn. Moreover, when the content of Pr reached 0.1 wt.%, plenty of Sn−Pr compounds were found in the Sn−9Zn solder. The inevitable oxidation of Sn−Pr compounds would cause a high stress accumulated within PrSn3 phases, which would be served as driving force to induce the Sn whisker sprout and growth after aging treatment at 150°C for 120 h to 360 h. Compared with the results in Sn−9Zn−0.5Ga−0.7Pr solder that Sn whisker observed until the addition of Pr reached 0.7 wt.%, it could be inferred that the addition of Ga may react against the sprout of Sn whisker.Originality/value: It is found that the addition of Pr can improve the properties of solder and avoid Sn whisker growth in the right range and proper conditions. The cost of the solder with added Pr is limited to RMB 2 yuan/kg so it can be widely used in industry.Keywords
This publication has 12 references indexed in Scilit:
- Reliability studies of Sn–9Zn/Cu and Sn–9Zn–0.06Nd/Cu joints with aging treatmentMaterials & Design (1980-2015), 2012
- Interfacial microstructure and bonding strength of Sn–3Ag–0.5Cu and Sn–3Ag–0.5Cu–0.5Ce–xZn solder BGA packages with immersion Ag surface finishMicroelectronics Reliability, 2011
- Sn whisker growth in Sn–9Zn–0.5Ga–0.7Pr lead-free solderJournal of Alloys and Compounds, 2011
- Properties and microstructure of Sn-9Zn lead-free solder alloy bearing PrJournal of Materials Science: Materials in Electronics, 2010
- Effects of rare earth element Nd on the solderability and microstructure of Sn–Zn lead-free solderJournal of Materials Science: Materials in Electronics, 2010
- Effect of plating temperature on Sn surface morphologyMaterials Letters, 2010
- Hollow tin/chromium whiskersApplied Physics Letters, 2010
- Effect of temperature on microstructural changes of the Sn–9wt.% Zn lead-free solder stripe under current stressingMaterials Chemistry and Physics, 2009
- Effects of Ga, Al, Ag, and Ce multi-additions on the properties of Sn–9Zn lead-free solderJournal of Materials Science: Materials in Electronics, 2009
- Spontaneous whisker growth on lead-free solder finishesMaterials Science and Engineering: A, 2005