Microstructure and pitting corrosion of similar and dissimilar stainless steel welds
Authors:
- G. M. ReddyGRG. M. Reddy
- K. S. RaoKRK. S. Rao
- T. SekharTST. Sekhar
- 1 May 2008
- journal article
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 13 (4) , 363-377
Abstract
Pitting Corrosion behaviour of similar and dissimilar metal welds of three classes of stainless steels, namely, austenitic stainless steel (AISI 304), ferritic stainless steel (AISI 430) and duplex stainless steel (AISI 2205), has been studied. Three regions of the weldment, i.e. fusion zone, heat affected zone and unaffected parent metal, were subjected to corrosion studies. Electron beam and friction welds have been compared. Optical, scanning electron microscopy and electron probe analysis were carried out to determine the mechanism of corrosion behaviour. Dissimilar metal electron beam welds of austenitic–ferritic (A–F), ferritic–duplex (F–D) and austenitic–duplex stainless steel (A–D) welds contained coarse grains which are predominantly equiaxed on austenitic and duplex stainless steel side while they were columnar on the ferritic stainless steel side. Microstructural features in the central region of dissimilar stainless steel friction welds exhibit fine equiaxed grains due to dynamic recrystallisation as a result of thermomechanical working during welding and is confined to ferritic stainless steel side in the case of A–F, D–F welds and duplex stainless steel side in the case of D–A welds. Beside this region bent and elongated grains were observed on ferritic stainless steel side in the case of A–F, D–F welds and duplex stainless steel side in the case of D–A welds. Interdiffusion of elements was significant in electron beam welding and insignificant in friction welds. Pitting corrosion has been observed to be predominantly confined to heat affected zone (HAZ) close to fusion boundary of ferritic stainless steel interface of A–F electron beam and D–F electron beam and friction weldments. The pitting resistance of stainless steel electron beam weldments was found to be lower than that of parent metal as a result of segregation and partitioning of alloying elements. In general, friction weldments exhibited better pitting corrosion resistance due to lower incidence of carbides in the microstructure.Keywords
This publication has 13 references indexed in Scilit:
- Microstructure and corrosion behaviour of alloy 690–SUS 304L butt joints formed by electron beam weldingScience and Technology of Welding and Joining, 2006
- Factors affecting initiation of pitting corrosion in super martensitic stainless steel weldmentsScience and Technology of Welding and Joining, 2001
- Characteristics of dissimilar welding of alloy 690 to 304L stainless steelScience and Technology of Welding and Joining, 2001
- Investigation of boundaries and structures in dissimilar metal weldsScience and Technology of Welding and Joining, 1998
- Friction welding of StAl and AlCu materialsJournal of Materials Processing Technology, 1995
- Influence of microstructure and composition on mechanical properties of some AISI 300 series weld metalsInternational Materials Reviews, 1993
- Correlation between solidification parameters and weld microstructuresInternational Materials Reviews, 1989
- Environmental cracking of type 316 austenitic stainless steel weldments in high temperature co2 gasMetallurgical Transactions A, 1988
- On the Mechanism of Localized Corrosion of Iron and Stainless SteelJournal of the Electrochemical Society, 1972
- Relation Between Anodic Dissolution And Resistance to Pitting CorrosionCorrosion, 1965