In this study, long-term reliability tests for high-power-density photovoltaic (PV) modules were introduced and analyzed in accordance with IEC 61215 and light-combined damp heat cycles, such as DIN 75220. The results indicated that post light soaking procedure, light-combined damp heat cycles caused a 3.51% power drop, while IEC standard tests (DH1000 and TC200) caused only 0.87% and 1.32% power drops, respectively. IEC 61215 failed to assess the long-term reliability of the high-power-density PV module, such as the passivated emitter rear cell. Additionally, based on the combined test, the latent heat () of the module was introduced to predict its degradation rate and to fit the prediction curve of the product guaranteed by the PV module manufacturers. facilitates in predicting a PV module’s lifespan according to the environmental factors of the actual installation area. The values of the PV stations in water environments, such as floating and/or marine PVs, indicated that they would last 7.2 years more than those on a rooftop, assuming that latent heat is the only cause of deterioration. Therefore, extending module life and improving power generation efficiency by determining installation sites to minimize latent heat would be advantageous.
Keywords
This publication has 22 references indexed in Scilit:
- Power performance of high density photovoltaic module using energy balance model under high humidity environmentSolar Energy, 2021
- The rapidly reversible processes of activation and deactivation in amorphous silicon heterojunction solar cell under extensive light soakingJournal of Materials Science: Materials in Electronics, 2021
- A practical optical and electrical model to estimate the power losses and quantification of different heat sources in silicon based PV modulesRenewable Energy, 2018
- Device physics underlying silicon heterojunction and passivating‐contact solar cells: A topical reviewProgress in Photovoltaics: Research and Applications, 2018
- Possible Candidates for Impurities in mc‐Si Wafers Responsible for Light‐Induced Lifetime Degradation and RegenerationSolar RRL, 2017
- Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22 %Energy Procedia, 2017
- Impact of the firing temperature profile on light induced degradation of multicrystalline siliconPhysica Status Solidi (RRL) – Rapid Research Letters, 2016
- Degradation and regeneration in mc‐Si after different gettering stepsProgress in Photovoltaics: Research and Applications, 2016
- Review of light-induced degradation in crystalline silicon solar cellsSolar Energy Materials and Solar Cells, 2016
- Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristicsSolar Energy Materials and Solar Cells, 2014