Recycling of Polyethylene into Strong and Tough Earth-Based Composite Building Materials
- 1 February 2016
- journal article
- research article
- Published by American Society of Civil Engineers (ASCE) in Journal of Materials in Civil Engineering
- Vol. 28 (2)
Abstract
Polyethylene (PE) waste often piles up in the environment for up to 30 to 50 years, without complete degradation. This paper describes how PE waste can be used as a reinforcement in laterite bricks for sustainable building materials. The bricks are produced with different volume percentages (0–30 vol. %) of PE. The flexural/compressive strengths and fracture toughness values of the composite blocks are compared with those of mortar (produced from river sand and cement). The composite containing 20 vol. % of PE is shown to have the best combination of flexural/compressive strength and fracture toughness. The flexural/compressive strengths and fracture toughness values increase with increasing volume percentage of PE up to 20 vol. %, before decreasing to minimum values for composites with 30 vol. % of PE. The trends in the measured strengths and fracture toughness values are explained using composite and crack bridging models.Keywords
This publication has 34 references indexed in Scilit:
- Laterite Based Stabilized Products for Sustainable Building Applications in Tropical Countries: Review and Prospects for the Case of CameroonSustainability, 2011
- Influence of cracking clays on satellite observed and model simulated soil moistureEGUsphere, 2010
- Mechanical properties of sisal fibre reinforced urea-formaldehyde resin compositesExpress Polymer Letters, 2007
- Biological degradation of synthetic polyesters—Enzymes as potential catalysts for polyester recyclingProcess Biochemistry, 2006
- Effects of reinforcement morphology on the fatigue and fracture behavior of MoSi2/Nb compositesActa Materialia, 1996
- Perspective on the Development of High‐Toughness CeramicsJournal of the American Ceramic Society, 1990
- Polymer Science Before and After 1899: Notable Developments During the Lifetime of Maurits DekkerJournal of Macromolecular Science: Part A - Chemistry, 1989
- Impact performance of sisal-polyester compositesJournal of Materials Science Letters, 1988
- Mechanisms of fatigue crack propagation in metals, ceramics and composites: Role of crack tip shieldingMaterials Science and Engineering: A, 1988
- Impact properties of natural fibre compositesJournal of Materials Science Letters, 1987