Hydrogen Solubility in Amorphous Silica at Pressures up to 75 kbar
- 18 December 2012
- journal article
- research article
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry B
- Vol. 117 (1) , 422-425
Abstract
The solubility of hydrogen in amorphous silica at a temperature of 250 °C and pressures up to 75 kbar is studied using a quenching technique. The molar ratio H2/SiO2 is found to linearly increase with pressure from X = 0.16 at P = 6 kbar to X = 0.53 at P = 75 kbar. An investigation of a sample with X = 0.47 by Raman spectroscopy demonstrated that hydrogen dissolves in silica in the form of H2 molecules, and these molecules occupy voids of, at least, two different types in the silica network. An X-ray diffraction study showed that the hydrogen molecules penetrating in the silica glass network prevented its irreversible densification occurring if the silica glass is compressed to the same pressure without hydrogen.Keywords
This publication has 14 references indexed in Scilit:
- New phase in the water–hydrogen systemJournal of Alloys and Compounds, 2011
- Helium penetrates into silica glass and reduces its compressibilityNature Communications, 2011
- Hydrogen formation observed during high pressure treatment of silica glassJournal of Non-Crystalline Solids, 2011
- Effect of helium on structure and compression behavior of SiO 2 glassProceedings of the National Academy of Sciences, 2011
- 3. Solar System Formation and Early Evolution: the First 100 Million YearsEarth, Moon, and Planets, 2006
- Solubility, diffusivity and trapping of hydrogen in dilute alloys. Deformed and amorphous metals—IIActa Metallurgica, 1982
- The interstitial structure of vitreous silicaJournal of Non-Crystalline Solids, 1978
- Molecular diffusion and solubility of hydrogen isotopes in vitreous silicaJournal of Applied Physics, 1977
- Raman scattering from hydrogen and deuterium dissolved in silica as a function of pressureJournal of Applied Physics, 1976
- Pressure dependence of helium and neon solubility in vitreous silicaJournal of Applied Physics, 1976