Headspace solid‐phase microextraction with gas chromatography/mass spectrometry reveals a correlation between the degradation product pattern and changes in the mechanical properties during the thermooxidation of in‐plant recycled polyamide 6,6
- 9 October 2002
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 86 (13) , 3396-3407
Abstract
The increased susceptibility of in‐plant recycled polyamide 6,6 toward thermooxidation was shown by headspace solid‐phase microextraction with gas chromatography/mass spectrometry (HS‐SPME/GC‐MS), tensile testing, differential scanning calorimetry (DSC), and Fourier transform infrared spectroscopy (FTIR). A correlation between the deterioration in mechanical properties and the formation of degradation products due to thermooxidation was found, and the most prominent decrease in mechanical properties coincided with the largest increase in the abundance of degradation products. The recycled materials had a shorter induction period toward oxidation, and their mechanical properties deteriorated faster than the mechanical properties of virgin material. The same trend was observed with HS‐SPME/GC‐MS because degradation products were found for recycled materials after oxidation times shorter than those for virgin material. Furthermore, larger amounts of degradation products were formed in the recycled materials. The high sensitivity of HS‐SPME/GC‐MS as an analytical tool was demonstrated because it was able to detect changes caused by oxidation considerably earlier than the other methods. Unlike DSC and FTIR, it could also show differences between samples recycled for different times. Four groups of degradation products—cyclic imides, pyridines, chain fragments, and cyclopentanones—were identified in thermooxidized polyamide 6,6. After 1200 h of thermooxidation, 1‐pentyl‐2,5‐pyrrolidinedione was the most abundant degradation product. Approximately four times more 1‐pentyl‐2,5‐pyrrolidinedione was formed in polyamide recycled three times than in virgin polyamide. Pyridines and chain fragments behaved toward oxidation and repeated processing like cyclic imides; that is, their amounts increased during oxidation, and larger amounts were formed in recycled materials than in virgin material. The cyclopentanone derivatives were present already in unaged material, and their amounts decreased during oxidation. Cyclopentanones were not formed because of the thermooxidation of polyamide 6,6. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 3396–3407, 2002Keywords
This publication has 30 references indexed in Scilit:
- Resonance Raman Studies of Photoinduced Decomposition of Nylon-6,6: Product Identification and Mechanistic DeterminationMacromolecules, 2000
- Rapid (bio)degradation of polylactide by mixed culture of compost microorganisms—low molecular weight products and matrix changesPolymer, 2000
- Photo-oxidative degradation of nylon 66 under accelerated weatheringPolymer, 1998
- Dicarboxylic Acids and Ketoacids Formed in Degradable Polyethylenes by Zip Depolymerization through a Cyclic Transition StateMacromolecules, 1997
- Thermal and Oxydative Stability of PVA and Nylon 6,6International Journal of Polymeric Materials and Polymeric Biomaterials, 1994
- FT–IR spectroscopic study on the thermal and thermal oxidative degradation of nylonsJournal of Polymer Science Part A: Polymer Chemistry, 1987
- FT–IR spectroscopic study on the photo‐ and photooxidative degradation of nylonsJournal of Polymer Science Part A: Polymer Chemistry, 1987
- Mechanism of thermal decomposition of nylon 66Macromolecules, 1987
- Analysis of polymers by pyrolysis/chemical ionization mass spectrometryJournal of Polymer Science: Polymer Chemistry Edition, 1982
- Mechanism of the Photoöxidation of AmidesJournal of the American Chemical Society, 1959