Structure and optical properties of tungsten thin films deposited by pyrolysis of W(CO)6 at various temperatures

Authors:

Abstract
Tungstenthin films, 200 nm thick, have been chemically vapor deposited by pyrolysis of W(CO)6 on oxidized silicon substrates at atmospheric pressure and temperatures varying from 350 to 500 °C. The structure of the films has been studied with x‐ray‐diffraction measurements and it was found that at depositiontemperature of 350 °C a face‐cubic‐centered phase is formed with a unit‐cell dimension of 0.4111 nm. At higher temperatures, up to 450 °C, the depositedfilms crystallize in a body‐cubic‐centered phase of tungsten with a unit cell of 0.317 nm. The complex dielectric constant (ε=ε1+iε2) of the films has been measured with spectroscopic ellipsometry within the energy range 1.5–6.5 eV. The energy variation of ε1 changes with depositiontemperature; instead, that of ε2 does not change significantly with it. The energy variation of ε1 for the filmsdeposited at temperatures below 400 °C corresponds to that of insulators while that of filmsdeposited at higher temperatures, up to 450 °C, reveals their metallic character.

This publication has 9 references indexed in Scilit: