Kinetics of Thermal Oxidation of Silicon Nitride Powders

Authors:

Abstract
The kinetics of thermal oxidation of H. C. Starck M‐11 and Ube SN‐E10 Si 3 N 4 powders was evaluated in the temperature range 650°‐1200°C using isothermal and nonisothermal thermogravimetric analysis, high‐resolution transmission electron microscopy, and X‐ray photoelectron spectroscopy. Between 700° and 1200°C, the isothermal kinetics was modeled equally well using the Ginstling‐Brounshtein and Zuravlev‐Lesokhin‐Tempeľman equations. Despite their similar particle sizes and surface areas, the two powders exhibited different oxidation kinetics. The activation energies for oxidation of the M‐11 and SN‐E10 powders were determined to be 400 and 540 kJ/mol, respectively, between 1000° and 1200°C, and 230 and 260 kJ/mol, respectively, between 700° and 1000°C. The parabolic rate constants for oxidation of the two powders were comparable to those reported in the literature for monolithic, chemically‐vapor‐deposited Si 3 N 4 at the higher temperatures. At lower temperatures, the oxidation kinetics of the M‐11 powder was nearly linear, whereas the kinetics of the SN‐E10 powder remained power‐law dependent.

This publication has 18 references indexed in Scilit: