New V45Zr20Ni20Cu10Al2.5Pd2.5 Glassy Alloy Powder with Wide Supercooled Liquid Region
Authors:
Open Access
- 1 January 2002
- journal article
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 43 (4) , 770-772
Abstract
New multicomponent V-based glassy alloy powder has been synthesized by mechanical alloying a mixture of elemental V45Zr20Ni20Cu10Al2.5Pd2.5 powder at room temperature, using a low energy ball mill. The glassy powder of the end-product (720 ks) in which its glass transition temperature (Tg) lies at a rather high temperature (745 K), crystallizes through two sharp exothermic reactions at 843 K and 919 K, respectively. The total enthalpy change of crystallization (ΔHx) is −1.78 kJ/mol. The supercooled liquid region before crystallization, ΔTx of the synthesized glassy powder shows a high value (98 K) for a metallic glassy system. The reduced glass transition temperature (ratio between Tg and liquidus temperatures, Tl (Tg⁄Tl)) was found to be 0.52.Keywords
This publication has 2 references indexed in Scilit:
- Preparation and Magnetic Properties of Co-based Bulk Glassy AlloysMATERIALS TRANSACTIONS, 2001
- New Fe–Co–Ni–Zr–B Amorphous Alloys with Wide Supercooled Liquid Regions and Good Soft Magnetic PropertiesMaterials Transactions, JIM, 1997