Effect of Pretreatment Process on Scale Formation in the Re-Boiler Section of Monoethylene Glycol Regeneration Plant
Open Access
- 7 June 2019
- conference paper
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 495 (1) , 012106
Abstract
Monoethylene glycol (MEG) regeneration plants often use pretreatment vessels to precipitate divalent cations, such as Fe 2+ , Ca 2+ , and Mg 2+ , in order to avoid or reduce fouling in downstream reboilers and heat exchangers. This pretreatment process operates under alkaline conditions and moderate temperatures (~ 80 °C) to accelerate the formation of lowsolubility divalent salts. The objective of the present research was to determine whether the pretreatment process could be minimized, without negatively impacts on the MEG regeneration process from to the formation of scale on the heater bundle in the presence of low concentrations of divalent cations in the rich MEG stream. Scale formation was analyzed under MEG regeneration process conditions using a dynamic scale loop (DSL) test and verification experiments were performed in a MEG regeneration and reclamation pilot plant, both with and without pretreatment conditions. The scaling tendencies of several rich MEGbrine mixtures were evaluated at different pH pretreatment levels and dissolved CO2 concentrations. An evaluation temperature of 180 °C was chosen to match the skin temperature of the reboiler heater bundle during the MEG regeneration process. The experiments of pH 7.24 showed high amounts of precipitation scale within the reboiler due to high remaining concentrations of mineral ions. In addition, small concentrations of calcium and magnesium ions led to the precipitation of calcite, dolomite, and magnesium hydroxide on the reboiler bundle and within associated filtered outputs even when a pretreatment vessel was present. These results were confirmed by the differential pressure build-up and Scanning Electron Microscopy analyses for each experimental condition. Another interesting finding is that pH increased within the reboiler due to CO2 gas boiling off at high operating temperatures, thus contributing to increased alkalinity levels, which in turn promoted scale formation. These results indicate that pretreatment should not be reduced, even with divalent ion concentrations as low as ~ 5 ppm TDS, due to the harsh conditions within the reboiler heater bundle.Keywords
This publication has 43 references indexed in Scilit:
- Carbonates precipitation in MEG loops – A comparative study of South Pars and Bass Strait gas fieldsJournal of Natural Gas Science and Engineering, 2015
- Effect of pH and Phosphate on Calcium Carbonate Polymorphs Precipitated at near-Freezing TemperatureCrystal Growth & Design, 2015
- Laboratory Methods for Scale Inhibitor Selection for HP/HT Fields2014
- Calcium Carbonate Scale Formation in Pipes: Effect of Flow Rates, Temperature, and Malic Acid as Additives on the Mass and Morphology of the ScaleProcedia Chemistry, 2014
- Calcium Carbonate Scale Formation, Prediction and Treatment (Case Study Gumry Oilfield-PDOC)International Letters of Chemistry, Physics and Astronomy, 2013
- Effects of Monoethylene Glycol on Carbonate Equilibrium and Calcite Solubility in Gas/Monoethylene Glycol/NaCl/Water Mixed SystemsSPE Journal, 2010
- Modeling of the Mixed Solvent Electrolyte System CO2−Na2CO3−NaHCO3−Monoethylene Glycol−WaterIndustrial & Engineering Chemistry Research, 2009
- Prediction of Scale Inhibitor Squeeze and Return in Calcite-Bearing Formation2005
- Calcium carbonate solubility: a reappraisal of scale formation and inhibitionTalanta, 1996
- The solubilities of calcite, aragonite and vaterite in CO2-H2O solutions between 0 and 90°C, and an evaluation of the aqueous model for the system CaCO3-CO2-H2OGeochimica et Cosmochimica Acta, 1982