Abstract
The stress corrosion cracking (SCC) of a commercial austenitic stainless steel, Type 304 (UNS S30400), has been investigated as a function of sensitizing temperature (800 K to 1,300 K) and test temperature (333 K to 373 K) in 0.82 kmol/m2 hydrochloric acid (HCl) solution using a constant load method. The three parameters were measured as a function of applied stress (σ), time-to-failure (tf), steady-state elongation rate (l˙ss), and transition time (tss, the time when the elongation starts to deviate from linearity before final failure). Curves for the sensitized specimens were divided into three regions that were dominated by either stress, SCC, or general corrosion. In the SCC-dominated region, the logarithm of l˙ss, which is obtained from the elongation vs time curve, is a linear function of the logarithm of tf, irrespective of σ and test temperature, although the slope depends upon sensitizing temperature. This result implies that l˙ss could be a useful parameter for the prediction of tf for sensitized as well as for solution-annealed specimens. Furthermore, the maximum applied stress in the SCC-dominated region, the value of tss/tf and the fracture mode (transgranular or intergranular), were found to depend upon sensitizing temperature. Results obtained are qualitatively discussed in terms of the interaction between the film formed at crack tips and grain boundary sliding (GBS), Cr carbides, and the grain boundary Cr depletion zone.