Effects of crystallinity and molecular weight on crack behavior in crystalline poly(L‐lactic acid)
Authors:
- 13 June 2011
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 122 (3) , 1976-1985
Abstract
The crack behavior and spherulitic morphology in melt‐crystallized poly(L‐lactic acid) (PLLA) were found to be molecular weight (MW) and crystallinity dependent, along with other key factors. With increasing MW in PLLA, the size of spherulites, band spacing of ring‐banded spherulites, and degree of crystallinity decreased, whereas cracks were increasingly less likely to occur. Multiple types of cracks, that is, circumferential and/or radial cracks, were massively present in low‐MW PLLA (PLLA‐11k), which had a high crystallinity. Upon cooling, in PLLA‐11k at most crystallization temperatures (Tc's), cracks formed, and the crack patterns were dependent on the lamellar morphology within the spherulites. Hexagonal, rather than circular, cracks occurred spontaneously during the cooling process of PLLA of a medium‐MW grade (PLLA‐120k) in PLLA film samples crystallized only at high Tc (135–138°C) and cooled to ambient temperature. However, no cracks of any types at all were present in PLLA films of high enough MWs (PLLA‐152k and PLLA‐258k) upon either slow air cooling or quench cooling when the samples were dipped into liquid nitrogen. Apparently, cooling‐induced contraction differences in different directions were invalid or not sufficient to address the complex cracking behavior in PLLA. In addition, for PLLA‐11k with a substantially high crystallinity, cracks were so prone to occur that even cover constraint imposed another factor in determining the crack and ring‐band patterns. More plausible mechanisms and correlations between the cracks, MW, crystallinity, spherulite size, and spherulite lamellar patterns of PLLA were analyzed in detail and proposed in this study. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011.Keywords
This publication has 16 references indexed in Scilit:
- Solvent Induced Cracking and Morphology in Banded Spherulite of Poly(trimethylene terephthalate)Polymer Journal, 2008
- Morphology and melt crystallization of poly(L‐lactide) obtained by ring opening polymerization of L‐lactide with zinc catalystPolymer Engineering & Science, 2006
- Cracking in polylactide spherulitesJournal of Polymer Science Part B: Polymer Physics, 2005
- Effect of PEG–PLLA diblock copolymer on macroporous PLLA scaffolds by thermally induced phase separationBiomaterials, 2004
- Recent Developments in Ring Opening Polymerization of Lactones for Biomedical ApplicationsBiomacromolecules, 2003
- Stresses and cracks in spherulites from transformation strainsScripta Materialia, 1996
- Cracking in spherulites of poly(hydroxybutyrate)Polymer, 1996
- Preparation and properties of absorbable fibres from l-lactide copolymersPolymer, 1993
- Thermal expansion and spherulite cracking in 3-hydroxybutyrate/3-hydroxyvalerate copolymersJournal of Materials Science Letters, 1989
- The relationship between microstructure and mode of fracture in polyhydroxybutyrateJournal of Polymer Science Part B: Polymer Physics, 1986