Effect of shade and thickness on the microhardness of resin-based composite specimens at different points considering curing light beam’s inhomogeneity
Open Access
- 30 July 2024
- journal article
- research article
- Published by Springer Nature in BMC Oral Health
- Vol. 24 (1) , 1-8
Abstract
Background: Recent studies have reported the inhomogeneity in the light emitted by dental light-curing units (LCUs). It is essential to understand how this uneven light distribution affects the physical properties of resin-based composites (RBCs) at various points across their surfaces. This study aimed to evaluate the effect of LCU beam’s inhomogeneity on the microhardness of RBCs with different shades and thicknesses. Methods: Four body (A1B, A2B, A3B, and A4B), one dentin (A3D), and one enamel shade (A3E) of RBC (Filtek Z350 XT) were examined. The specimens were fabricated in four thicknesses (1, 2, 3, and 4 mm) and subjected to a 40-second light-curing. Vickers microhardness testing was performed at the center point, and 3 mm left and right from the center at the bottom surface of each sample. The LCU beam profile was characterized using a beam profiler, while irradiance after specimen passage was measured using a spectrometer. One-way analysis of variance (ANOVA) and Tukey’s post-hoc tests were used to analyze the effects of shades and thicknesses on irradiance and microhardness, respectively. One-way repeated-measures ANOVA was used to compare the microhardness across different points. Pearson’s correlation analysis examined the relationship between irradiance and microhardness. Results: The beam profile of LCU revealed inhomogeneous light distribution. Light irradiance was decreased with both the increase in thickness and darker shade of the specimens (p < 0.05). Microhardness was found to decline with an increase in sample thickness (p < 0.05), and was consistently higher at the center point compared to the periphery, particularly in thicker (3 and 4 mm) and darker shades (A3B, A4B, and A3D). A positive correlation was found between the irradiance and microhardness across all evaluated points (p < 0.05). Conclusions: Inhomogeneous light emission from LCU significantly influences the microhardness of RBC samples, depending on the thicknesses and shades. The findings underline the importance of considering LCU beam inhomogeneity in clinical settings to ensure optimal polymerization of RBC.Keywords
All Related Versions
Funding Information
- Korea Medical Device Development Fund (RS-2020-KD000044)
This publication has 28 references indexed in Scilit:
- Homogeneity of dental curing unit beam profile and its effect on microhardness of dental composites with varying thicknessesDental Materials, 2022
- Effect of light curing units on the polymerization of bulk fill resin-based compositesDental Materials, 2018
- Effect of the irradiance distribution from light curing units on the local micro-hardness of the surface of dental resinsDental Materials, 2015
- Correlation between the beam profile from a curing light and the microhardness of four resinsDental Materials, 2014
- Post-cure depth of cure of bulk fill dental resin-compositesDental Materials, 2014
- Polymerization kinetic calculations in dental composites: a method comparison analysisClinical Oral Investigations, 2013
- Depth of cure of resin composites: Is the ISO 4049 method suitable for bulk fill materials?Dental Materials, 2012
- New insight into the “depth of cure” of dimethacrylate-based dental compositesDental Materials, 2012
- Translucency, opalescence and light transmission characteristics of light-cured resin compositesDental Materials, 2010
- Effects of finishing and polishing procedures on the surface texture of resin compositesDental Materials, 1994