Crack Detection during Laser Metal Deposition by Infrared Monochrome Pyrometer
Open Access
- 10 December 2020
- Vol. 13 (24) , 5643
Abstract
Laser metal deposition (LMD) is an advanced technology of additive manufacturing which involves sophisticated processes. However, it is associated with high risks of failure due to the possible generation of cracks and bubbles. If not identified in time, such defects can cause substantial losses. In this paper, real-time monitoring of LMD samples and online detection of cracks by an infrared monochrome pyrometer (IMP) could mitigate this risk. An experimental platform for crack detection in LMD samples was developed, and the identification of four simulated cracks in a 316L austenitic stainless-steel LMD sample was conducted. Data at temperatures higher than 150 °C were collected by an IMP, and the results indicated that crack depth is an important factor affecting the peak temperature. Based on this factor, the locations of cracks in LMD-316L austenitic stainless-steel samples can be determined. The proposed technique can provide real-time detection of cracks through layers of cladding during large-scale manufacturing, which suggests its relevance for optimizing the technological process and parameters, as well as reducing the possibility of cracks in the LMD process.Keywords
Funding Information
- Ministry of Science and Technology of China (2018YFB1105302)
This publication has 54 references indexed in Scilit:
- Defects monitoring of laser metal deposition using acoustic emission sensorThe International Journal of Advanced Manufacturing Technology, 2016
- Improving Non-Destructive Concrete Strength Tests Using Support Vector MachinesMaterials, 2015
- 3D-imaging of selective laser melting defects in a Co–Cr–Mo alloy by synchrotron radiation micro-CTActa Materialia, 2015
- Vision-based defect detection in laser metal deposition processRapid Prototyping Journal, 2014
- Laser Additive Manufacturing in Surface Modification of Metals2014
- Cracking behavior and mechanical properties of austenitic stainless steel parts produced by laser metal depositionMaterials & Design (1980-2015), 2013
- Laser Additive ManufacturingPhotonicsViews, 2010
- Crack growth micro-mechanisms in the IN718 alloy under the combined influence of fatigue, creep and oxidationInternational Journal of Fatigue, 2009
- Laser Beam Build-Up Welding: Precision in Repair, Surface Cladding, and Direct 3D Metal DepositionJournal of Thermal Spray Technology, 2007
- Analysis and design considerations for a real-time system for non-destructive evaluation in the nuclear industryUltrasonics, 1982