Boron doping of silicon using coalloying with aluminium
Authors:
- 28 November 1994
- journal article
- Published by AIP Publishing in Applied Physics Letters
- Vol. 65 (22) , 2792-2794
Abstract
We present a new technique for boron (B) doping of silicon. In this letter we show that a B doping profile of more than 2 μm thickness with a maximum active doping concentration of 3×1019 cm−3 can be formed by a fast (<1 min) alloying process at a temperature of 850 °C. Thick-film aluminum is used to obtain an alloying and epitaxial regrowth process in accordance with the Al–Si phase diagram. The atomic concentration profile of the B- and Al-doped Si layer was determined by secondary ion mass spectrometry. The active doping concentration was measured with an automatic electrochemical capacitance/voltage profiler. By the addition of B to the Al paste, the epitaxially regrown layer is doped with B and Al to the solid solubility of these elements in Si at the particular regrowth temperature. The applicability of this fast low temperature B doping process in Si solar cell processing is discussed.Keywords
This publication has 1 reference indexed in Scilit:
- The Al-Si (Aluminum-Silicon) systemBulletin of Alloy Phase Diagrams, 1984