Development of Facets, Spirals, and Etch Pits on Copper Crystals by Heating to High Temperatures in High Vacua

Authors:

Abstract
Single crystal spheres of OFHC and 99.999% copper were heated to temperatures of 950 to 1075° in high vacua. In the case of the OFHC copper, facets parallel to the (111), (110), and (100) planes were formed over relatively large areas centered at the respective poles, and with some of these crystals spiral facets were formed around the (111) pole. When an OFHC crystal was heated in a copper cup, an appreciable number of pits were formed. In the case of the 99.999% copper, facets parallel to the (111) and (100) planes were formed in small areas around the respective poles, and at certain temperatures etch pits were formed. An attempt was made to interpret the difference in the size of the facets formed on the two types of crystals in terms of the influence of impurities on the rates of evaporation. It was proposed that the etch pits formed at dislocations in the crystal, although there was not a one-to-one correspondence between pits and dislocations.

This publication has 9 references indexed in Scilit: