Viscoelastic Behaviour of Wood Fibres during the Hot Pressing of Medium Density Fibreboard
Authors:
- J. van HoutsJHJ. van Houts
- D. BhattacharyyaD. Bhattacharyya
- K. JayaramanKJK. Jayaraman
- 26 June 2003
- journal article
- Published by Walter de Gruyter GmbH in Holzforschung
- Vol. 57 (4) , 391-399
Abstract
Summary Sufficient stress relaxation within a medium density fibreboard (MDF) mat during hot pressing is critical for producing a panel with acceptable mechanical properties and dimensional stability. This paper describes a series of load relaxation tests of wood fibres conducted at temperatures and moisture contents similar to those within an MDF mat during the hot pressing process (temperatures ranging from 80°C to 100°C with relative humidity levels ranging from 9% to 68%). The results clearly show an increase in relaxation when either the temperature or relative humidity is increased. The relaxation behaviour of MDF is also measured and the trends observed are comparable to those of the wood fibres. Taguchi experimental design is employed to analyse the effects of temperature, moisture content and initial stress on the viscoelastic behaviour of MDF.Keywords
This publication has 3 references indexed in Scilit:
- Determination of Residual Stresses in Medium Density FibreboardHolzforschung, 2000
- The Hot Pressing of Dry-formed Wood-based Composites - Part VI. The Importance of Stresses in the Pressed Mattress and their Relevance to the Minimisation of Pressing Time, and the Variability of Board PropertiesHolzforschung, 1989
- Relaxation behaviour of the amorphous components of woodJournal of Materials Science, 1987