Variable-dose (1017–1020 cm−3) phosphorus ion implantation into 4H–SiC

Authors:

Abstract
Multiple-energy box profile elevated-temperature (700 °C) phosphorus ion implantations were performed into 4H–SiC in the doping range of 1×1017–1×1020 cm−3. The implanted material was annealed at 1500, 1600, or 1650 °C with an AIN encapsulant to prevent degradation of the SiC surface. Within this temperature range the sheet resistance does not change significantly for a given dose. The percentage of electrical activation of the P donors initially decreased with increasing implant dose for P-implant concentration up to 3×1019 cm−3 and then increased again at higher doses. For 1×1020 cm−3 P implant, a carrier concentration of 4×1019 cm−3 was measured at room temperature. In the 1017 cm−3 P doping concentration range substitutional activation greater than 85% was measured. Despite performing the implants at 700 °C, a significant amount of as-implanted damage was observed in the Rutherford backscattering (RBS) spectrum, even for 1018 cm−3 range P implantations. The RBS yield after annealing is near the virgin level for P concentrations up to 1×1019 cm−3, but above this concentration the RBS yield is above the virgin level, indicating a significant amount of residual lattice damage in the crystal.

This publication has 26 references indexed in Scilit: