Influence of Processing on the Mechanical Properties of Ti-6Al-4V-Based Composites Reinforced with 7.5 mass% TiC and 7.5 mass% W
Authors:
- 1 January 2008
- journal article
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 49 (9) , 2153-2158
Abstract
No abstract availableThis publication has 32 references indexed in Scilit:
- Laser fabrication of Ti6Al4V/TiC composites using simultaneous powder and wire feedMaterials Science and Engineering: A, 2007
- Microstructure and mechanical properties of highly deformed Ti–6Al–4VMaterials Science and Engineering: A, 2005
- Effect of tungsten additions on the mechanical properties of Ti-6Al-4VMaterials Science and Engineering: A, 2005
- Micro/nanoscale mechanical and tribological characterization of SiC for orthopedic applicationsJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2004
- Effect of thermal oxidation on corrosion and corrosion–wear behaviour of a Ti–6Al–4V alloyBiomaterials, 2004
- Microstructure and mechanical properties of severely deformed powder processed Ti–6Al–4V using equal channel angular extrusionScripta Materialia, 2003
- Microstructure and mechanical properties of Ti/W and Ti–6Al–4V/W composites fabricated by powder-metallurgyMaterials Science and Engineering: A, 2003
- Implant Applications of Highly Corrosion-Resistant Ti-15Zr-4Nb-4Ta AlloyMATERIALS TRANSACTIONS, 2002
- Titanium alloys in total joint replacement—a materials science perspectiveBiomaterials, 1998
- Abrasive wear of intermetallic-based alloys and compositesMaterials Science and Engineering: A, 1997