Effect of Preheating Temperature on Microstructure and Properties of 42CrMo4/38MnVS6 Heterogeneous Laser Welded Joint
Open Access
Abstract
Laser-welded forged steel pistons can meet the needs of the new era of heavy truck engines. 42CrMo4 and 38MnVS6 are widely used as piston materials due to the good mechanical properties. This study investigates the influence of preheating on microstructure and mechanical properties of 42CrMo4/38MnVS6 laser welding joint. The experimental results show preheating increases the laser absorption capacity of the metal, which can lead to an increase in weld width. The microstructure of weld is the high-hardness and poor toughness twin martensite without preheating. As the temperature of preheating increases, the twin martensite in the weld begins to transform into lath martensite and regenerates ferrite and bainite. As the preheating temperature increases, the plane fracture toughness (K1C) of the weld increases and then decreases, reaching the highest value of 2322.94 MPa·mm−1/2 at 150 °C. Compared with no preheating conditions, the tensile strength of the welded joint after preheating is improved. The fracture mode of welded joints changes from brittle fracture to ductile fracture. When the preheating temperature is 100–200 °C, the tensile strength of the welded joint reaches 1018.1–1032.5 MPa; when the preheating temperature is 250 °C–300 °C, the tensile strength decreases.Keywords
This publication has 15 references indexed in Scilit:
- New MAHLE Steel Piston and Pin Coating System for Reduced TCO of CV EnginesSAE International Journal of Commercial Vehicles, 2016
- Formation and influence mechanism of keyhole-induced porosity in deep-penetration laser welding based on 3D transient modelingInternational Journal of Heat and Mass Transfer, 2015
- Heat treatment of welded joints of steel 0.3С–1Cr–1Si produced by high-power fiber lasersOptics & Laser Technology, 2015
- The effect of preheat & post weld heat treatment on the laser weldability of AISI 420 martensitic stainless steelMaterials & Design (1980-2015), 2014
- Direct Friction Welding of TiAl Alloy to 42CrMo Steel RodsMaterials and Manufacturing Processes, 2014
- Failure Analysis of HAZ Cracking in Low C–CrMoV Steel WeldmentJournal of Failure Analysis and Prevention, 2009
- Residual stresses and fracture mechanics analysis of a crack in welds of high strength steelsEngineering Fracture Mechanics, 2007
- Effects of welding processes on the mechanical properties of HY 80 steel weldmentsMaterials & Design (1980-2015), 2007
- Welding characteristics of S45C medium carbon steel in laser welding process using a high power CW Nd:YAG laserJournal of Materials Science, 2004
- Weldability characteristics of shielded metal arc welded high strength quenched and tempered platesJournal of Materials Engineering and Performance, 2002