Characteristics of Cavitation Erosion Using Image Processing Techniques
- 20 December 2012
- journal article
- Published by ASME International in Journal of Tribology
- Vol. 135 (1) , 014502
Abstract
This paper deals with the analysis of eroded surfaces obtained from cavitation-erosion experiments on stainless steel in water and oil-in-water (o/w) emulsions using image processing. Two analysis techniques that are very promising in this respect are the wavelet decomposition transform and fractals. These can be used to extract parameters that characterize the cavitation intensity in a similar manner to that of the mean depth of erosion (MDP). The extracted parameters are the wavelet energy and entropy as well as the fractal dimension. Both of the image feature parameters and the MDP decrease with adding oil to water. Also, it was found that the variation of image feature parameters versus concentration of oil-in-water emulsions has a general trend that does not depend on magnification factor. The cavitation erosion behavior and mechanism for water and o/w emulsions were analyzed and it was found that the predominant failure mode was fatigue for water and o/w emulsions. The results show that a corrosive effect appears at 5 and 10 wt% o/w emulsions.Keywords
This publication has 28 references indexed in Scilit:
- Fractal Analysis of Cavitation Eroded Surface in Dilute EmulsionsJournal of Tribology, 2011
- Investigation Into Cavitation Erosion PitsJournal of Tribology, 2009
- Characterizing cavitation erosion particles by analysis of SEM imagesTribology International, 2009
- Quantitative Analysis of Cavitation Erosion Particle Morphology in Dilute EmulsionsJournal of Tribology, 2008
- Cavitation Erosion Mechanism Based on Analysis of Erosion ParticlesJournal of Tribology, 2008
- Analysis of Tribochemical Surface Damage by Image Processing (Analysis of Tribochemical Damages)Tribology Letters, 2002
- Investigation of the temperature effects on induced impact pressure and cavitation erosionWear, 1998
- Fatigue failure of SUS 304 caused by vibratory cavitation erosionWear, 1994
- Cavitation erosion of iron and steelMetallurgical Transactions A, 1978
- Cavitation erosion of age-hardenable aluminum alloysMetallurgical Transactions A, 1978