Abstract
An adsorption thermodynamic model of the oxidation of Ni-Cr alloys is proposed. According to this model, the adsorption of the alloy component with a lower surface energy (Ni) at the alloy-oxide film interface shifts the equilibrium of the solid-phase reaction 3NiO + 2Cr = Cr2O3 + 3Ni (1) toward the enrichment of the oxide film in NiO. It was demonstrated that the total Gibbs energy change for reaction (1) can be presented as ΔG T, S = ΔG T + ΔG S, where ΔG T < 0 is the contribution from the Gibbs energy of the thermochemical reaction of oxidation of Ni and Cr atoms and ΔG S > 0 is the contribution from the surface Gibbs energy of formation of the alloy associated with the replenishment of the surface layer of the alloy during its oxidation. Calculations of ΔG S are based on the published data on the surface energy of the pure metal ΔG S o and results of authors’ theoretical studies. It was found that the dependence of ${{a_{NiO}^3 } \mathord{\left/ {\vphantom {{a_{NiO}^3 } {a_{Cr_2 O_3 } }}} \right. \kern-0em} {a_{Cr_2 O_3 } }}$ on the content of Cr in the alloy determined from calculated equilibrium characteristic of reaction (1) at 1373 K proved to be in satisfactory agreement with the available experimental data on the composition of the oxide film on Ni-Cr alloys. In addition, the values of the potentials of metal-oxide Ni and Cr electrodes in an aqueous solution at 298 K are calculated, which nearly coincide with the published values of the Flade potential for the passivation of these metals.

This publication has 5 references indexed in Scilit: