The Dependence of Secondary Dendrite Arm Spacing on Solidification Conditions—II. Al-7 Si-0.5 Mg Alloys treated with Sr and Sb
Authors:
- 1 March 1993
- journal article
- research article
- Published by Taylor & Francis in Cast Metals
- Vol. 6 (1) , 42-46
Abstract
Steady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrite arm spacing which can be described by the equations: for Sr treated alloys and for Sb treated alloys where tf is the total solidification time. Specimens quenched during solidification are used to follow the coarsening of secondary dendrite arms during solidification. It is shown that coarsening behaviour can be described by an average coarsening parameter, , in the equation If the geometrical constant B is assumed to be 33, the value of calculated from spacing measurements is 20.80 and 15.22 (μm s−1) for Sr- and Sb-treated alloys, respectively. Both additions reduce the rate of coarsening. The influence of the additions on the growth temperatures of the primary Al phase and the eutectic phase is discussed.Keywords
This publication has 2 references indexed in Scilit:
- Quantitative Description of the Microstructure of Aluminium Foundry AlloysCast Metals, 1991
- Growth of interdendritic eutectic in directionally solidified Al-Si alloysMetallurgical Transactions A, 1987