Abstract
B‐doped Si1−xGex layers with Ge fractions, determined by Rutherford backscattering spectroscopy, ranging from 0 to 0.28 and B concentrations, from quantitative secondary‐ion spectroscopy measurements, between 5×1016 and 4×1019 cm−3 were grown on Si(001) at temperatures Ts=475–575 °C by gas‐source molecular beam epitaxy from Si2H6, Ge2H6, and B2H6. Film thicknesses ranged from 200 nm for alloys with x=0.28 to 800 nm with x=0.05 to 1.4 μm for Si. Structural analyses by high‐resolution x‐ray diffraction and reciprocal lattice mapping combined with transmission electron microscopy showed that all films were fully strained, with measured relaxations of only ≂4×10−5, and exhibited no evidence of dislocations or other extended defects. The hole conductivity mobility μc,h in these layers increased continuously with increasing Ge concentrations, whereas the Hall mobility decreased yielding a Hall scattering factor that ranged from 0.75 for Si to 0.26 for Si0.72Ge0.28 but was not strongly affected by B concentration. μc,h, with CB=2×1018 cm−3, varied from 110 cm2 V−1 s−1 for Si0.95Ge0.05 to 158 cm2 V−1 s−1 for Si0.72Ge0.28, compared to 86 cm2 V−1 s−1 for Si, in good agreement with Boltzmann transport model calculations accounting for changes in the valence‐band structure due to the effects of both alloying and biaxial in‐plane compressional strain.

This publication has 58 references indexed in Scilit: