Influence of Strain on the Environmental Hydrogen-Assisted Cracking of a High-Strength Steel in Sodium Chloride Solution
Authors:
- 1 March 1988
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 44 (3) , 176-185
Abstract
Evidence is presented that will establish the role of mechanical strain in promoting surface absorption of hydrogen by rupturing surface films on AISI(1) 4340 steel in alkaline 3.5% sodium chloride solution. Such bare surface generation is shown to substantially influence the alloy’s hydrogen cracking susceptibility. The effect of strain-enhanced absorption is reported for smooth, tapered, and notched tensile specimens under slowly straining conditions and is also shown to explain hydrogen-assisted cracking behavior for double cantilever beam fracture mechanics specimens with pre-existing fatigue cracks. The interrelationship between slow continuous straining at a given strain rate to produce a minimum critical strain for film rupture and the associated time will be shown to be a critical factor for this system in all specimen types. Enhancement of hydrogen absorption per unit area of bare surface created with film removal, as determined by Devanathan-Stachurski hydrogen permeation measurements, explain the effect. Additional evidence based upon interpretation of permeation distances and the dimensions of the crack tip plastic zone suggests that the rate determining hydrogen transport step for hydrogen-assisted cracking of AISI 4340 steel in alkaline seawater is hydrogen absorption.Keywords
This publication has 42 references indexed in Scilit:
- Hydrogen transport during deformation in nickel: Part II. Single crystal nickelMetallurgical Transactions A, 1986
- The Importance of Transient Effects Resulting from Dislocation Transport of Hydrogen1983
- Evidence for Dislocation Transport of Hydrogen in AluminumMetallurgical Transactions A, 1982
- Effects of hydrogen on the properties of iron and steelMetallurgical Transactions A, 1980
- Fracture mechanics and surface chemistry studies of subcritical crack growth in AISI 4340 steelMetallurgical Transactions A, 1978
- Sorption of tritium by nickel during plastic deformationMetallurgical Transactions A, 1976
- Hydrogen transport by dislocationsMetallurgical Transactions A, 1976
- A short-time diffusion correlation for hydrogen-induced crack growth kineticsMetallurgical Transactions A, 1975
- Stress history effect on incubation time for stress corrosion crack growth in AISI 4340 steelMetallurgical Transactions, 1972
- Effect of prestressing on the stress-corrosion resistance of two high-strength steelsMetallurgical Transactions, 1972