Thermal conductivity of poly(ether ether ketone) and its short‐fiber composites

Authors:

Abstract
The effects of crystallinity, orientation, and short‐fiber filler on the thermal diffusivity D and thermal conductivity K of poly (ether ether ketone) (PEEK) have been studied. Below the glass transition, D increases by less than 10% as the crystallinity increases from 0 to 0.3. For amorphous PEEK, there is an abrupt drop in D at the glass transition (Tg ⋍ 420 K). The drop is less prominent for the 30% crystalline sample and occurs at 20 K higher. At a draw ratio of 2.5, the axial thermal conductivity is 2.3 times higher while the transverse thermal conductivity is 30% lower than that of the unoriented material. For an injection‐molded bar of carbon fiber reinforced PEEK, the variation of D with position along the width or thickness direction is found to correlate well with the fiber orientation. By regarding the injection‐molded bar as a multidirectional laminate comprising a large number of unidirectional plies, the thermal conductivities along the longitudinal and transverse direction are calculated and found to agree closely with the experimental data. © 1994 John Wiley & Sons, Inc.

This publication has 13 references indexed in Scilit: