Optimization of atmospheric leaching parameters for cadmium and zinc recovery from low-grade waste by response surface methodology (RSM)
Authors:
Open Access
- 17 January 2024
- journal article
- research article
- Published by Springer Nature in Scientific Reports
- Vol. 14 (1) , 1-12
Abstract
This study is focused on the optimization of effective parameters on Cadmium and Zinc recovery by atmospheric acid leaching of low-grade waste by response surface methodology (RSM) and using the Central Composite Design (CCD) method. The effects of parameters including time (0.5–2.5 h), temperature (40–80 °C), solid/liquid (S/L) (0.05–0.09 g/cc), particle size (174–44 mic), oxygen injection (0–1%) and pH (0.5–4.5) were statistically investigated at 5 surfaces. The sample of low-grade waste used in this study was mainly zinc factory waste. Two quadratic models for the correlation of independent parameters for the maximum recovery were proposed. The properties of waste were evaluated by X-ray diffraction (XRD) and X-ray fluorescence (XRF). Atomic absorption spectroscopy was used to determine the amount of Cadmium and Zinc in the leaching solution. The correlation coefficient (R2) for the predicted and experimental data of Cadmium and Zinc are 0.9837 and 0.9368, respectively. Time, S/L and size were the most effective parameters for the recovery efficiency of cadmium and zinc. 75.05% of Cadmium and 86.13% of Zinc were recovered in optimal conditions of leaching: S/L 0.08, pH 2.5, size 88 µm, 70 °C and 2.5 h. with air injection.Keywords
This publication has 37 references indexed in Scilit:
- Alkaline leaching of lead and zinc by sodium hydroxide: kinetics modelingJournal of Materials Research and Technology, 2018
- Geogenic cadmium pollution and potential health risks, with emphasis on black shaleJournal of Geochemical Exploration, 2017
- Extraction of copper, zinc and cadmium from copper–cadmium‐bearing slag by oxidative acid leaching processRare Metals, 2016
- Preparation of high purity cadmium with micro-spherical architecture from zinc flue dustTransactions of Nonferrous Metals Society of China, 2015
- Leaching of cadmium, chromium, copper, lead, and zinc from two slag dumps with different environmental exposure periods under dynamic acidic conditionEcotoxicology and Environmental Safety, 2014
- Selective zinc alkaline leaching optimization and cadmium sponge recovery by electrowinning from cold filter cake (CFC) residueHydrometallurgy, 2012
- Leaching behavior of cadmium from hazardous wasteSeparation and Purification Technology, 2012
- Leaching of low grade zinc oxide ores in Ida2--H2O systemTransactions of Nonferrous Metals Society of China, 2011
- Recovery of cadmium from hydrometallurgical zinc smelter by selective leachingHydrometallurgy, 2010
- Determination of the optimum conditions for the leaching of Cd–Ni residues from electrolytic zinc plant using statistical design of experimentsSeparation and Purification Technology, 2008