Effect of increased charring on the narrow side of rectangular timber cross‐sections exposed to fire on three or four sides
Authors:
- 23 January 2011
- journal article
- research article
- Published by Wiley in Fire and Materials
- Vol. 35 (8) , 593-605
Abstract
Owing to the influence of two‐dimensional heat transfer, fire tests and heat transfer calculations show that charring on the narrow side of rectangular timber cross‐sections may be considerably greater than charring on the wide side. For timber members unprotected throughout the time of fire exposure as well as members initially protected from fire exposure, it is shown by calculation, that the relationship between charring on the narrow side and time is nonlinear. In order to take into account increased charring on the narrow side of timber members a section factor ks was determined. By calculation it is shown that bending moment resistance is only insignificantly influenced by the effect of two‐dimensional heat transfer and the factor ks can therefore be neglected, making the fire design of timber members easier. Copyright © 2011 John Wiley & Sons, Ltd.Keywords
This publication has 7 references indexed in Scilit:
- Charring model for timber frame floor assemblies with void cavitiesFire Safety Journal, 2008
- Structural fire design according to Eurocode 5—design rules and their backgroundFire and Materials, 2004
- Modeling of the thermal degradation of structural wood members exposed to fireFire and Materials, 2004
- Charring rates and temperature profiles of wood sectionsFire and Materials, 2003
- Fire performance of timber constructionProgress in Structural Engineering and Materials, 2000
- Short communication: Temperature profiles in wood members exposed to fireFire and Materials, 1994
- Charring rate of wood for ASTM E 119 exposureFire Technology, 1992