Abstract
The characterization of Mn-doped 3C-SiC prepared by ion implantation is reported. Implantation of Mn ions at a dose of 1×1016cm−2 into a 3C-SiC homoepitaxial wafer was carried out. High temperature annealing following the implantation process was found to enhance the ferromagnetic ordering. Transmission magnetic circular dichroism and magnetization investigations demonstrated a ferromagnetic behavior below 245K . The lattice relaxation induced by the postannealing is considered a possible mechanism of this outcome.