Online Monitoring Systems of Microbiologically Influenced Corrosion on Cu-10% Ni Alloy in Chlorinated, Brackish Water
Authors:
- M. de RomeroMRM. de Romero
- Z. DuqueZDZ. Duque
- O. de RincónORO. de Rincón
- 1 August 2000
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 56 (8) , 867-876
Abstract
Alloy Cu-10% Ni (ASTM B-111, UNS C70600) has been used extensively for condenser and heat exchanger tubes in power stations. However, there have been cases of severe localized corrosion in this alloy. This paper presents the evaluation of Cu-10% Ni in a dynamic online monitoring system with one-way circulation using alkaline (pH 7.2 to pH 8.8) brackish water with and without chlorination for 3-, 8-, and 12-month exposure periods. Electrochemical laboratory tests—open-circuit potential (OCP), linear polarization resistance (LPR), and cyclic polarization (CP)—also were run. Before chlorination, the microbiological water analysis indicated microbial development with planktonic and sessile sulfate-reducing bacteria (SRB) on the order of 107 cells/mL and 105 cells/mL, respectively, with sessile SRB at 10 cells/mL after chlorination. Prechlorination scanning electron microscopy (SEM)/ energy dispersive x-ray (EDX) analysis/x-ray diffraction (XRD) analysis after 3 months revealed very few cuprite (Cu2O) crystals and bacterial cells, whereas dense cell populations associated with hemispheric holes typical of microbiologically influenced corrosion (MIC) were found after 8 months. Postchlorination SEM/EDX/XRD analysis helped establish a definition of how chlorine increases the Cu-10% Ni corrosion rate. Initially, a dense layer of star-shaped Cu2O crystals was observed. It later was removed partly because it quickly oxidized into nonprotective, nonadherent secondary corrosion products, which again exposed the material to the hypochlorite ions in the corrosive medium, consequently forming a new layer of Cu2O. The formation of different corrosion products and redeposited copper with severe localized corrosion below the deposits and severe general corrosion finally were shown by the analysis of a tube that was in service for 3 years in the same chlorinated, brackish water. CP curves indicated that chlorine content increased the corrosion current from 2.5 μA/cm2 per 0.0 ppm Cl2 to 5.0 μA/cm2 per 0.3 ppm Cl2, and that Cu-10% Ni is not passivated in this brackish water. All these results suggest that this alloy is not corrosion resistant in brackish water, and chlorine treatment accelerates corrosion even more.Keywords
This publication has 6 references indexed in Scilit:
- Microbiologically Influenced Corrosion of Copper in Ground Water1999
- Microbiologically Influenced Corrosion Handbook1994
- Microbiologically Influenced Corrosion of Copper Alloys in Saline Waters Containing Sulfate-Reducing Bacteria1991
- A technical review of electrochemical techniques applied to microbiologically influenced corrosionCorrosion Science, 1991
- A Morphological Study of Pitting Corrosion of Copper in Soft Tap WaterCorrosion, 1989
- Influence of Biofouling and Biofouling Control Techniques on Corrosion of Copper-Nickel Tubes1983